Tensile Failure of Tungsten-Nickel-Cobalt

ORAL

Abstract

Spall experiments were conducted on a 91W-Ni-Co alloy. The spall strength was 2.6~GPa. At 410 m/s, which is well above the spall strength, the damage consists of isolated voids. The failure starts mainly as grain cleavage. This result is very consistent with earlier measurements in which very rapid tensile failure was induced by transverse impact.