Optical Vortexed Transmission through a Nanoslit on the Pyramid
ORAL
Abstract
The nanoslit apertures with its gap ranging from 1 nm to $\sim $ 50 nm have been fabricated using microfabrication process such as wet etching, thermal oxidation, circular aperture opening by HF, then followed by Al metal deposition. The light transmission through the single nanoslit apertures has been measured to be dependent upon the gap between two metal edges and independent of length of the slit. With decreasing the gap from 80 nm to 1 nm, the optical transmission rate has been increased upto three order of magnitude. This can be attributed to optical vortexed transmission
*This research has been funded by the National Research Lab project of KOSEF.
–